1940 Knuckle Cases
When cases have been welded and I see some porosity . . . I like to paint the inside with glyptal red and bake them. I tape 'em off all nice. They look swell on the bench. When this old, cast aluminum heats up - oil can work it's way through the pores and make a mess of your engine - unless you like the well-worn look ?